[1]张盈盈,韩文礼,高进伟,等.HFW焊管沟槽腐蚀敏感性评价方法的研究[J].石油管材与仪器,2018,4(05):55-57.[doi:10.19459/j.cnki.61-1500/te.2018.05.016]
             ZHANG Yingying,HAN Wenli,GAO Jinwei,et al.Evaluation Methods of HFW Weld Groove Corrosion Sensitivity[J].Petroleum Tubular Goods & Instruments,2018,4(05):55-57.[doi:10.19459/j.cnki.61-1500/te.2018.05.016]
            点击复制

            HFW焊管沟槽腐蚀敏感性评价方法的研究
            分享到:

            《石油管材与仪器》[ISSN:2096-0077/CN:61-1500/TE]

            卷:
            4
            期数:
            2018年05期
            页码:
            55-57
            栏目:
            试验研究
            出版日期:
            2018-10-20

            文章信息/Info

            Title:
            Evaluation Methods of HFW Weld Groove Corrosion Sensitivity
            文章编号:
            2096-0077(2018)05-0055-03
            作者:
            张盈盈1韩文礼1高进伟2周冰1曹杉2孔祥领2陈利红3
            1.中国石油集团工程技术研究院 天津 300451;2.中国石油技术开发公司 ?#26412;?100028;3.天津东义镁制品股份有限公司 天津 301721
            Author(s):
            ZHANG Yingying1 HAN Wenli1 GAO Jinwei2 ZHOU Bing1 CAO Shan2 KONG Xiangling2 CHEN Lihong3
            1.CNPC Research Institute of Engineering Technology, Tianjin 300451,China;2.China Petroleum Technology & Development Corporation, Beijing 100028,China;3.Tianjin Dongyi Magnesium Products Co. Ltd., Tianjin 301721,China
            关键词:
            HFW焊管沟槽腐蚀三维激光扫描
            Keywords:
            HFW pipegroove corrosionthreedimensional laserscanning
            分类号:
            TG162.83
            DOI:
            10.19459/j.cnki.61-1500/te.2018.05.016
            文献标志码:
            A
            摘要:
            焊缝沟槽腐蚀敏感性采用恒电位加速腐蚀法进行评价。在评价沟槽腐蚀的最深深度时,目前是采用线性切割、磨金相、再利用金相显微镜观察的方法进行。在切割和磨金相的过程中,对腐蚀坑深度影响较大,从而使测量存在较大的人为误差。试验使用三维激光扫描仪原位测量了沟槽的腐蚀深度,简化了试验步骤,并且减少了人为误差。
            Abstract:
            The potentiostatic accelerated corrosion method is used to evaluate the groove weld corrosion susceptibility of HFW pipe. When evaluating the deepest trench depth of corrosion, a linear cutting and grinding metallurgical are currently used, and then the trench depth is observed by optical microscopy. During cutting and grinding metallurgical process, the corrosion pit depth is impacted seriously, and the artificial error is large. Threedimensional laser scanner insitu measurement is used to analyze the trench corrosion depth, this method simplifies the testing procedures, and reduces the artificial error.

            参考文献/References:

            [1] ?#29486;?#23731;,任永峰,井小天.微电极扫描法对HFW焊缝沟槽腐蚀敏感性研究[J]. 焊管,2011,34(10):5-8.
            [2] 王玮,齐慧滨,肖光成,等.ERW焊管沟槽腐蚀行为研究与评价[J]. 世界钢铁,2007,7(6):20-24.
            [3] 邬中华.X52直缝焊管沟槽腐蚀评价方法的研究[J]. 太钢科技,2009,20(3):33-37.
            [4] 石荣满,刘书国.ERW钢管的沟状腐蚀及结果分析[J]. 防腐保温技术,2004,12(4):6-11.
            [5] 曹楚南.腐蚀电化学原理(第三版)[M]. ?#26412;?#21270;学工业出版社,2008.

            相似文献/References:

            [1]胡美娟,邵春明,池强,等.凸台焊接对HFW焊管性能影响的模拟研究[J].石油管材与仪器,2018,4(02):45.[doi:10.19459/j.cnki.61-1500/te.2018.02.012]
             HU Meijuan,SHAO Chunming,CHI Qian,et al.Simulation Research on the Influence of Outlet Fitting Welding to HFW Welded Pipe[J].Petroleum Tubular Goods & Instruments,2018,4(05):45.[doi:10.19459/j.cnki.61-1500/te.2018.02.012]

            备注/Memo

            备注/Memo:
            第一作者简介:张盈盈,女,1978年生,高级工程师,2005年毕业于华中科技大学应用化学专业,目前主要从事油气田储罐、管线腐蚀与防护的研究。E-mail:[email protected]