[1]趙金蘭.鋼管管體拉伸試驗中屈強比的計算與判定探討[J].石油管材與儀器,2018,4(05):75-77.[doi:10.19459/j.cnki.61-1500/te.2018.05.022]
             ZHAO Jinlan.Calculation and Judgment of Yield Ratio in Steel Tube Tensile Test[J].Petroleum Tubular Goods & Instruments,2018,4(05):75-77.[doi:10.19459/j.cnki.61-1500/te.2018.05.022]
            點擊復制

            鋼管管體拉伸試驗中屈強比的計算與判定探討
            分享到:

            《石油管材與儀器》[ISSN:2096-0077/CN:61-1500/TE]

            卷:
            4
            期數:
            2018年05期
            頁碼:
            75-77
            欄目:
            標準化
            出版日期:
            2018-10-20

            文章信息/Info

            Title:
            Calculation and Judgment of Yield Ratio in Steel Tube Tensile Test
            文章編號:
            2096-0077(2018)05-0075-03
            作者:
            趙金蘭
            中國石油集團石油管工程技術研究院 陜西 西安 710077
            Author(s):
            ZHAO Jinlan
            CNPC Tublular Goods Research Institute, Xi′an, Shaanxi 710077, China
            關鍵詞:
            管體拉伸試驗屈強比數值修約極限數值判定
            Keywords:
            tube tensile test yield ratio numerical values judgment of limiting values
            分類號:
            TE973
            DOI:
            10.19459/j.cnki.61-1500/te.2018.05.022
            文獻標志碼:
            A
            摘要:
            通過對GB/T 9711-2017和API Spec 5L-2018,以及相關引用標準的對比分析,針對目前國內在鋼管力學性能試驗中存在的不一致情況,探討了管體拉伸試驗屈強比的計算步驟、試驗數值的修約程序和極限數值的判定方法,同時評述了GB/T 8170-2008和ASTM E29-2004的實用性。
            Abstract:
            In view of the inconsistencies presented in the current domestic steel pipe mechanical properties tests, the calculation steps of the yield ratio in the tensile test of steel pipe body, the rounding procedure of the test data and the decision method of the threshold limits value are discussed by comparing the GB/T 9711-2017 and API Spec 5L-2018 with the related references. Then the practicality of GB/T 8170-2008 and ASTM E29-2004 are further reviewed.

            參考文獻/References:

            [1] 機械工業理化檢驗人員技術培訓和資格鑒定委員會. 力學性能試驗[M]. 北京:中國計量出版社,2008:32.
            [2] 鋼鐵研究總院等. 金屬材料 拉伸試驗 第一部分:室溫試驗方法:GB/T 228.1-2010[S]. 北京:中國標準出版社,2011:1.
            [3] 美國材料與試驗協會ASTM. 鋼產品力學性能試驗方法和定義Standard Test Methods and Definitions for Mechanical Testing of Steel Products:ASTM A 370-2014[S]. 美國材料與試驗協會ASTM,2014:附錄A8.
            [4] 美國材料與試驗協會ASTM. 用試驗數據的有效數字確定符合標準要求的實施方法Standard Practice for Using Significant Digits in Test Data to Determine Conformance with Specifications:ASTM. ASTM E29-2004[S]. 美國材料與試驗協會ASTM,2004:2-4.
            [5] 中國標準化研究院等. 數值修約規則與極限數值的表示和判定:GB/T 8170-2008[S]. 北京:中國標準出版社,2008:1-4.
            [6] 寶雞石油鋼管有限責任公司等. 石油天然氣工業管線輸送系統用鋼管:GB/T 9711-2017[S]. 北京:中國標準出版社,2017:1.
            [7] 寶雞石油鋼管有限責任公司(鋼管研究院).管線鋼管規范Specification for Line Pipe:API Spec 5L -2018[S]. 石油工業標準化研究所翻譯出版2018:1.

            備注/Memo

            備注/Memo:
            第一作者簡介:趙金蘭,女,1982年生,工程師,2009年畢業于中國礦業大學(北京),獲碩士學位,目前主要從事石油管道技術支持工作, E-mail:[email protected]